Recommended slicer setting:
retraction speed over 80MM/S
retraction length 2.5-4MM
If you are facing PLA clogging problem, please try the followings:
1. Increase the retraction speed. The speed may have being limited in the firmware try to change it. G-command "M203 E200"
2. Increase the extruder acceleration. Check your firmware settings. G-command "M201 E9000"
3. Reduce the retraction length. It depends on your machine setup.
4. Increase the nozzle temperature by 5-10 degrees.
5. Do not install the 2 screws for support the heatblcok like the stock hotend on the CR-10 printer.
6. Make sure that there is no gap between the heatsink and the heat breaker.
NOTE:
This product only supports 1.75mm filament!!!
We found that many customers do not know how to properly install the nozzle.
Remember the core issues in the installation process.
Just make sure your nozzle and HEAT BREAK front end are tight and sealed. Otherwise, the filament will leak along the screw holes.
Packing list:
High quality MK8 Brass Nozzle 1.75/0.4mm x 1
Titanium alloy heat break 1.75MM x 1
High quality Aluminum Heater Block x 1
Aluminium Heatsink x 1
Thermistor (NTC 100K B3950 can be up to 300 degrees) x 1
Heater Cartridge(12V 40W) x 1
Silicone socks x 1
Finally: