3D Printer Platform Upgraded Gold Pattern Build Plate for BambuLab A1 X1C X1 X1E P1P P1S: Smooth Hexagonal Honeycomb+ Plaid Hologram Dual Sided Flexible Spring Steel Sheet 257x257mm

KWD 8.500
KWD 9

Brand
Imdinnogo
Weight
300 g
1 +

Special Features

  • Double Sides Selection: one side has a hexagonal honeycomb pattern, texture brightly colored, emitting a different light, the other side has a check pattern, the bottom of the model will show vivid motifs. adding more interesting inspirations to your creations and immersing you in the fun of Bamboo 3D printing project
  • No magnticc sticker, size: 257×257mm/10.1×10.1inch. Suitable fo Bambu Lab X1 X1C X1-Carbon X1E P1P P1S A1, not for A1 Mini 3d printer. Please confirm your 3D printer hotbed size before ordering
  • Buildplate is removable and can be bent to remove the model quickly, without the help of other tools. Please let the build plate cool down before remove the model. Unlike H1H/PEI/PEO/PEY/PET printing hotbed surfaces, we recommend the use of glue stick for better adhesion
  • Easy Maintenance: For better adhesion, clean well. Use well with isopropylalcoho and wipe with a lint free towel between each print. Any bit of oil or residue will make the print non-stick
  • Print bed surface can withstand high temperature, supports various 1.75mm filaments, such as PLA, PETG, ABS, TPU. And the suggested temperature is PLA: 60-65℃; PETG: 70-90℃; ABS: 90-100℃

Description

Package Includes:
1Pcs 257mm double sides coating steel plate

We recommend filament use temperature:
PLA: Heat bed temperature60-65℃ / 140-149℉ and 220-230 ℃ / 428-446 ℉ in the nozzle.
PETG: Heat bed temperature 70-90℃ / 158-194℉, nozzle temperature 240-250 ℃ / 464-482 ℉.
ABS: Hot bed temperature 90-100℃/194-212℉, nozzle temperature 250-270 ℃/482-518 ℉.
IF YOUR PRINTER IS X1/XIC/X1E,
PLEASE TURN OFF "ENABLEDETECTION OF BUILD PLATE POSITION": Before choosing a plate type: 1. OPEN "BAMBU STUDIO"; 2. Click "Device"; Click "Print Options"; 3. Uncheck "Enable detection of build plate position".
Excellent adhesion for first printing layer
The levelling nozzle should not be set too low, because if the nozzle cuts into the platform, it may cause permanent damage, or if the first layer is too low, it may cause too strong adhesion, resulting in the pick-up die tearing off the top layer.

Related Items


{"error":"Error","cart_limit":"You have too many items in your cart.","prod_limit":"You cannot add any more of this item"}